first POM print

A project log for High-voltage assisted 3d printing

Attempting to use high voltage for better adhesion to print bed

deepsoicDeepSOIC 03/09/2016 at 22:150 Comments

It was a disaster. two seconds after being deposited, the trace peels itself off the bed..

Data:

bed: ITO glass @ 140 deg.C, high voltage off

extruder 250 C

--

other observations:

POM melts at 150 C. It is a true melting point: below, it's unextrudable; above - it extrudes fairly well.